Descripción
| Clasificaciones: | EN ISO 16834-A, G 69 3 M Mn3Ni1CrMo, EN ISO 16834-A, G Mn3Ni1CrMo, Wire Electrode, SFA/AWS A5.28, ER100S-G, Wire Electrode |
| Aprobaciones: | CE, EN 13479, DB, 42.039.18, VdTÜV, 04436 |
Aprobaciones vinculadas a la planta de producción. Para obtener más información, pongase en contacto con ESAB.
| Alloy Type: | Low alloyed (1.4 % Ni, 0.3 % Cr, 0.3 % Mo) |
Análisis del Metal de Soldadura
Propiedades de Ensayo de impacto Charpy
| EN 80Ar/20CO2 (M21) As welded | |||
| Impact Value | Testing Temperature | Stress Relieved Testing Temp | Stress Relieved Testing Time |
| 100 J | 20 °C | – | – |
| 70 J | -20 °C | – | – |
| 60 J | -30 °C | – | – |
| EN 80Ar/20CO2 (M21) Stress relieved | |||
| Impact Value | Testing Temperature | Stress Relieved Testing Temp | Stress Relieved Testing Time |
| 130 J | 20 °C | 620 °C | 15 hr |
| 60 J | -20 °C | 620 °C | 15 hr |
| 60 J | -30 °C | 620 °C | 15 hr |
Typical Tensile Properties
| AWS 80Ar/20CO2 (M21) As welded | ||||
| Elongation | Tensile Strength | Yield Strength | Stress Relieved Temperature | Stress Relieved Testing Time |
| – | – | – | – | – |
| EN 80Ar/20CO2 (M21) As welded | ||||
| Elongation | Tensile Strength | Yield Strength | Stress Relieved Temperature | Stress Relieved Testing Time |
| 19 % | 820 MPa | 730 MPa | – | – |
| EN 80Ar/20CO2 (M21) Stress relieved | ||||
| Elongation | Tensile Strength | Yield Strength | Stress Relieved Temperature | Stress Relieved Testing Time |
| 20 % | 750 MPa | 690 MPa | 620 °C | 15 hr |





Valoraciones
No hay valoraciones aún.